crackyourinterview.com


To improves our performance please Like Share Subscribe(Will boost us)

A casting defect which occurs due to improper venting of sand is known as
Question Posted on 06 Jan 2025Home >> Mechanical Engineering >> Workshop Technology >> A casting defect which occurs due to improper venting of sand is known as

A casting defect which occurs due to improper venting of sand is known as
Choose the correct option from below list
(1)shift
(2)blow holes
(3)swell
(4)cold shuts

Answer:-(2)blow holes
0
0




.


Most Visited Questions:-

Deep Learning Questions Answers
Below are the different Deep Leaning Questions and answer a More...

What is Gulpjs and some multiple choice questions on Gulp
Gulpjs is an open source whihc helps in building Javascript More...

Continuous Integration Questions Answers
Below are the 20 odd questions for CI or Continuous Integra More...

Derived relationships in Association Rule Mining are represented in the form of __________.
Derived relationships in Association Rule Mining are repres More...

Microservices Architecture Questions Answers
Below are the different questions on Microservices Architec More...




Other Important Questions

Structural sections such as rails, angles, I-beams are made by

The operation of cutting of a flat sheet to the desired shape is called

The temperature of the inner luminous cone of neutral flame is about

A casting defect which occurs due to improper venting of sand is known as

For obtaining a cup of diameter 25 mm and height 15 mm by drawing, the size of the round blank should be approximately






@2014-2022 Crackyourinterview (All rights reserved)